(20) Aluminum alloy (6061) (Al with 0.6 wt% Si and 1.0 wt% Mg) is subjected to age hardening 3. treatment. (a) (8) Plot...
Problem 4 (20 pts): An alloy was subjected to age hardening test at different precipitation heat treatment temperatures. Consider the graph shown below, relating the variation of yield strength of the tested alloy with the precipitation heat treatment durations. 1 min 1 h 1 day 1 month 1 year 70 121°C (250°F) 400 60 50 300 40 149°C (300°F) Yield strength (MPa) Yield strength (ksi) 200 30 204°C (400°F) 20 260°C (500°F) 10 100 0 SS 0 10-2 1 103...