Question 2 A titanium tube 200mm diameter and 5mm wall thickness is subjected to an internal pressure of 13.5MPa. The tube co

Question 3 For the above question if the crack is found to be 1mm deep to what pressure must the tube be subjected to cause f

Question 3 For the above question if the crack is found to be 1mm deep to what pressure must the tube be subjected to cause f


please answer both the questions

Question 2 A titanium tube 200mm diameter and 5mm wall thickness is subjected to an internal pressure of 13.5MPa. The tube contains a longitudinal crack along its full length. Assuming that the tube can be approximated by a single edge notched plate subjected to a tensile stress equal to the hoop stress in the tube determine the crack length to cause failure. You may assume that the material fracture toughness is 55 MPavm. Please provide your answer in mm Enter answer
Question 3 For the above question if the crack is found to be 1mm deep to what pressure must the tube be subjected to cause failure? Please provide your answer in MPa
0 0
Add a comment Improve this question Transcribed image text
Answer #1

DEOmm Pd 13. SX200 at tongtin failuer is ac CrRek ongsh e 70 O O132 Mm This is criHcal cyack lenth to failuer.Craek alepth Imm internial presg ure Craee Eloepl- T- P= 2tx T4 mm Yeilding in titenium 70 MPa P 10.8 MPa

Add a comment
Know the answer?
Add Answer to:
please answer both the questions Question 2 A titanium tube 200mm diameter and 5mm wall thickness...
Your Answer:

Post as a guest

Your Name:

What's your source?

Earn Coins

Coins can be redeemed for fabulous gifts.

Not the answer you're looking for? Ask your own homework help question. Our experts will answer your question WITHIN MINUTES for Free.
Similar Homework Help Questions
  • Question 2. (Total 18 marks) 350 350 300 300 Same plot, but with expanded x axis...

    Question 2. (Total 18 marks) 350 350 300 300 Same plot, but with expanded x axis 250 250 200 Stress (MPa) Stress (MPa) 150 $150 100 100 0 0 0 0.02 0.04 0.06 0.12 0.14 0.16 0.18 0 0.08 0.1 Strain 0.001 0.002 0.003 0.004 0.005 0.006 0.007 0.008 0.009 0.01 Strain (a) Determine the % elongation, yield stress and ultimate tensile strength of the material tested above (3 marks) (b) Calculate the elastic modulus of the material tested above...

  • Only answer question 2 please, it refers to question 1 that is why both are in the image.

    Only answer question 2 please, it refers to question 1 that is why both are in the image. 1. Identify the weibull modulus m and characteristic stress ơ0 from the series of fracture strength values 246, 191, 230, 350, 286, 206, 310, 150, 271, 133, 216, 265, 320, 176, 261,196, 251, 164, 100, and 229 (in MPa) that were measured by three-point bending of samples having length l- 30 mm, depth d - 5 mm, and height h 5 mm...

  • answer question 2 please A material may fail in many ways; in a ductile or brittle...

    answer question 2 please A material may fail in many ways; in a ductile or brittle mode; by creep or fatigue; by corrosion or stress corrosion; by hydrogen or liquid metal embrittlement; by slow tensile overload or by impact. An examination of the failure may tell you a lot about the material and the failure mode. In this course, you have learned (we trust) the correlations between structure-properties, - applications. This leads to material selection. However, the engineer has to...

ADVERTISEMENT
Free Homework Help App
Download From Google Play
Scan Your Homework
to Get Instant Free Answers
Need Online Homework Help?
Ask a Question
Get Answers For Free
Most questions answered within 3 hours.
ADVERTISEMENT
ADVERTISEMENT
ADVERTISEMENT