Annealing Temperature (°C)

Electrical Conductivity (ohm1? cm1)

Yield Strength (MPa)

Grain Size (mm)

400

3.04 × 105

86

0.10

500

3.05 × 105

85

0.10

600

3.36 × 105

84

0.10

700

3.45 × 105

83

0.098

800

3.46 × 105

52

0.030

900

3.46 × 105

47

0.031

1000

3.47 × 105

44

0.070

1100

3.47 × 105

42

0.120

Step-by-Step Solution

Request Professional Solution

Request Solution!

We need at least 10 more requests to produce the solution.

0 / 10 have requested this problem solution

The more requests, the faster the answer.

Request! (Login Required)


All students who have requested the solution will be notified once they are available.
Add your Solution
Textbook Solutions and Answers Search