Annealing Temperature Size (°C)

Residual Stresses (psi)

Tensile Strength (psi)

Grain Size (in.)

250

21,000

52,000

0.0030

275

21,000

52,000

0.0030

300

5000

52,000

0.0030

325

0

52,000

0.0030

350

0

34,000

0.0010

375

0

30,000

0.0010

400

0

27,000

0.0035

425

0

25,000

0.0072

Step-by-Step Solution

Request Professional Solution

Request Solution!

We need at least 10 more requests to produce the solution.

0 / 10 have requested this problem solution

The more requests, the faster the answer.

Request! (Login Required)


All students who have requested the solution will be notified once they are available.
Add your Solution
Textbook Solutions and Answers Search